Nanocrystalline α-Al2O3 powder was prepared through a chemical route via a reaction between aluminum nitrate nona hydrate with a sucrose template in variation ratios of the salt to the organic namely 1 : 2, 3 : 1, and 6 : 1 at a heating temperature of 200 oC. The homogenization process of the nanopowder was assisted by milling a"charcoal precursor" in a non polar solvent for 24 hours, which was then successfully calcined at temperatures of 900 oC and 1100 oC. The products were evaluated by X-ray diffraction (XRD) analysis, scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The optimum condition was obtained at a ratio of the aluminum salt to the organic compound of about 6 : 1, at a calcination temperature of 900 oC, which produced a 100% pure α-Al2O3 phase with a crystallite size of 44.6 nm. The SEM micrographs showed the particle sizes of nanocrystalline α-Al2O3 powders were found to be near 100 nm at 1100 oC. The TEM results indicate that nanocrystalline α-Al2O3 powders calcined at 900 oC had grain sizes below 50 nm. An increase of the sucrose concentration leads to smaller crystal sizes, meanwhile an elevation of the calcination temperature from 900 oC to 1100 oC leads to the formation of larger particle and crystal sizes of alumina.

Keywords: Nanocrystalline, Al2O3, Sucrose, A chemical process, Calcination temperature.

This Article

  • 2011; 12(4): 365-370

    Published on Aug 31, 2011