  • Residual strength and thermal stability of sustainable high-strength concrete using ceramic waste
  • Ma Xiangminga,* and Wang Zhigangb

  • aSchool of Civil Engineering, Chongqing Vocational Institute of Engineering, Chongqing, 402260, China
    bSchool of Materials Science and Engineering, Chongqing University, Chongqing, 400044, China

  • This article is an open access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/4.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.

References
  • 1. D. Tavakoli, M. Hashempour, A. Heidari, and Pertanika J. Sci. Technol. 26 (2018) 499-522.
  •  
  • 2. S.A. Zareei, F. Ameri, N. Bahrami, P. Shoaei, H.R. Musaeei, and F. Nurian, J. Build. Eng. 26 (2019) 100914.
  •  
  • 3. I. Guerra, I. Vivar, B. Llamas, A. Juan, and J. Moran, Waste Manage. 29 (2009) 643-646.
  •  
  • 4. C. Medina, M.I. Sanchez de Rojas, and M. Frias, Cem. Concr. Compos. 34[1] (2012) 48-54.
  •  
  • 5. S.Y. Mousavi, A. Tavakkoli, M. Jahanshahi, and A. Dankoub, Int. J. Eng. Trans. C Asp. 33 (2020) 1085-1093.
  •  
  • 6. V. Lopez, B. Llamas, A. Juan, J.M. Moran, and I. Guerra, Biosyst. Eng. 96[4] (2007) 559-564.
  •  
  • 7. P.S. Song, S. Hwang, and B.C. Sheu, Cement Concr. Res. 35[8] (2005) 1546-1550.
  •  
  • 8. A. Sotayo, S. Green, and G. Turvey, Environ. Technol. Innov. 3 (2015) 97-107.
  •  
  • 9. M. Ucar and Y. Wang, Int. J. Cloth. Sci. Technol. 23[4] (2011) 242-248.
  •  
  • 10. M.H. Khaneghahi, E.P. Najafabadi, P. Shoaei, and A.V. Oskouei, Polym. Test. 71 (2018) 72-86.
  •  
  • 11. H.R. Pakravan and F. Memarian, J. Ind. Text. 46[3] (2015) 833-851.
  •  
  • 12. B.S.S. Begum, R. Gandhimathi, S.T. Ramesh, and P.V. Nidheesh, J. Mater. Cycles Waste Manag. 15 (2013) 564-570.
  •  
  • 13. A.M. Kilic, O. Kilic, and M.O. Keskin, Sci. Res. Essays, 5[15] (2010) 1986-1992.
  •  
  • 14. K.V. Boobala Krishnan, K. Nirmalkumar, V. Sampathkumar, and P.C. Murugan, J. Ceram. Process. Res. 24[4] (2023) 714-722.
  •  

This Article

  • 2025; 26(4): 698-701

    Published on Aug 31, 2025

  • 10.36410/jcpr.2025.26.4.698
  • Received on Apr 9, 2025
  • Revised on Jun 9, 2025
  • Accepted on Jun 10, 2025

Correspondence to

  • Ma Xiangming
  • School of Civil Engineering, Chongqing Vocational Institute of Engineering, Chongqing, 402260, China
    Tel : +86 13648422638

  • E-mail: xiaomagemxm@163.com